GB/Z 41117-2021Fasteners - Fundamentals of hydrogen embrittlement in steel fasteners (English PDF)
紧固件 钢制紧固件氢脆基本原理
This is a limited preview
Buy now to download the full PDF (17 pages)
Need quotation for your management?
Get a formal quotation for GB/Z 41117-2021 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
December 31, 2021
Implementation date
December 31, 2021
Scope
GB/Z 41117-2021 is the English-translated version of 紧固件 钢制紧固件氢脆基本原理.
GB/Z 41117-2021 is a Chinese guidance document, identical to ISO/TR 20491:2019, that explains the fundamentals of hydrogen embrittlement in steel fasteners.
It describes the mechanisms of hydrogen damage, fracture morphology and crack tip conditions, then sets out the conditions for failure: material susceptibility, tensile stress and atomic hydrogen.
Further chapters look at case-hardened fasteners, thermal shock during hot dip galvanizing, stress relief before electroplating, thread rolling after heat treatment, test methods for hydrogen embrittlement and baking.
It is aimed at the whole fastener supply chain, from steel mills and fastener makers to coating suppliers, joint designers and end users, and applies to steel fasteners. It was issued on 31 December 2021.
Found what you need?
Document preview — GB/Z 41117-2021
National Standard of the People's Republic of China
- ICS
- 21.060.01
- Classification
- J 13
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- Preface
- Introduction
- 1 Scope
- 2 Normative references
- 3 Terms and Definitions
- 4 Abbreviations
- 5 General description of hydrogen embrittlement
- 6 Hydrogen damage mechanism
- 7 Fracture morphology
- 8 Crack tip condition
- 9 Hydrogen Embrittlement Failure Conditions
- 9.1 Root Causes and Predisposing Factors of Hydrogen Embrittlement Failure
- 9.2 Material Sensitivity
- 9.3 Tensile stress
- 9.4 Atomic Hydrogen
- 10 Case hardened fasteners
- 11 Hot dip galvanizing - effects of thermal shock
- 12 Stress relief before electroplating
- 13 Thread rolling after heat treatment of fasteners
- 14 Hydrogen embrittlement test method
- 15 Baking
Foreword
This document is in accordance with the provisions of GB/T 1.1-2020 "Guidelines for Standardization Work Part 1. Structure and Drafting Rules of Standardization Documents" drafted.
This document is equivalent to ISO /T R20491.2019 "Basic Principles of Hydrogen Embrittlement of Steel Fasteners for Fasteners".
The technical report is adjusted to my country's national standardization guiding technical document.
Introduction
High-strength steel fasteners generally refer to fasteners with tensile strength (Rm) exceeding 1000MPa, which are often used in bridges, engines, aerospace The failure of fasteners in these parts can have catastrophic consequences. Failure prevention and hydrogen embrittlement (HE) risk management are Fundamental issues that need to be considered in the entire fastener supply chain, including. steel mills, fastener manufacturers, surface coating suppliers, applications Engineers, connection designers to end users. Hydrogen embrittlement has been studied for decades, however, the complexity of the phenomenon and numerous variables make The occurrence of fastener failure is unpredictable. Relevant research is usually carried out under simplified and/or ideal conditions, and its conclusions are difficult to translate into Fastener industry standard or instructive production technology in practice. In addition, the differences between different norms and standards, some requirements are not sufficient Some requirements are too strict, which makes the situation more complicated. Inconsistencies and even contradictory standards in the fastener industry have led to many conjectures. confusion and avoidable fastener failures. Hydrogen embrittlement is often mistakenly seen as a source of failure rather than a failure mechanism. reflects this conceptual confusion. Fasteners Basic Principles of Hydrogen Embrittlement of Steel Fasteners
1 Scope
This document provides a brief and complete introduction to the latest knowledge on hydrogen embrittlement from a professional and technical point of view.
This document applies to steel fasteners.
2 Normative references
There are no normative references in this document.
3 Terms and Definitions
The following terms and definitions apply to this document.
3.1 Hardness
The resistance of a metal to plastic deformation, usually represented by an indentation or penetration of a solid (surface or core).
3.2 Work hardening
When the metal is plastically deformed (by rolling, drawing, drawing, thread rolling, heading, extrusion, etc:) at room temperature, the strength and hardness (3.1) increase, while The phenomenon of reduced ductility.
3.3 Heat treatment
The process of heating, holding and cooling metal materials or workpieces in an appropriate manner to obtain the desired structure and properties.
NOTE: Fastener heat treatment includes, but is not limited to, quenching and tempering, annealing, case hardening, and stress relief. [Source: GB/T 7232-2012, 2.1]
3.4 Quenching and tempering
Quenching and tempering quenching and tempering; QT.
The workpiece is heated to austenitize and then rapidly cooled to obtain a martensite (or bainite) structure, and then reheated to a certain temperature and maintained at a certain temperature.
Cool to room temperature after a period of time to obtain the desired physical or mechanical properties of the heat treatment (3.3) process.
3.5 Case hardening
Chemical heat treatment process consisting of carburizing or carbonitriding and quenching to increase the surface hardness (3.1) of steel fasteners.
Note: This process is used for self-tapping screws, self-extrusion screws and self-drilling self-tapping screws, etc.
3.6 Stress relief
The heat treatment (3.3) process of heating the fastener to an appropriate temperature and maintaining it for a certain period of time, and then slowly cooling it to reduce the Residual stresses due to hardening (3.2).
3.7 Baking
The process of heating fasteners at a specified temperature and time to reduce the risk of intrinsic hydrogen embrittlement (3.15).
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 17 pages — is available in the English PDF.
Similar standards
How to Download GB/Z 41117-2021
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/Z 102.17-2026 — Semiconductor devices - Discrete devices - Part 17: Magnetic and capacitive coupler for basic and reinforced insulation
GB/Z 103-2026 — Health informatics - The architecture of internet healthcare service network
GB/Z 108-2026 — Health informatics - Internet healthcare service pattern
GB/Z 41117-2021
$300.00