Scope
GB/T 35316-2017 is the English-translated version of 蓝宝石晶体缺陷图谱.
GB/T 35316-2017 is the Chinese standard "Collection of metallographs on defects of sapphire crystal". Its scope clause reads: This standard specifies the terms and definitions of sapphire crystal defects, morphology characteristics and causes.
This standard applies to the inspection and analysis of various defects in the preparation of sapphire single crystal materials. Its clauses include terms and definitions; sapphire crystal defects.
Found what you need?
Document preview — GB/T 35316-2017
National Standard of the People's Republic of China
- ICS
- 29.045
- Classification
- H 80
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- 1 Scope
- 2 Normative references
- 3 Terms and Definitions
- 4 Sapphire crystal defects
1 Scope
This standard specifies the terms and definitions of sapphire crystal defects, morphology characteristics and causes.
This standard applies to the inspection and analysis of various defects in the preparation of sapphire single crystal materials.
2 Normative references
The following documents are indispensable for the application of this document. For dated references, only dated versions apply to this article
Pieces. For undated references, the latest version (including all amendments) applies to this document.
GB/T 8756 crystal defect map
GB/T 14264 Semiconductor Material Terms
GB/T 30453 silicon raw material defect map
3 Terms and Definitions
The terms and definitions defined in GB/T 8756, GB/T 14264 and GB/T 30453 apply to this document.
4 Sapphire crystal defects
4.1 Ingot Defects
4.1.1 crack
4.1.1.1 Morphological features
The grown sapphire crystal is sometimes complete in shape, but several cracks can be observed inside or at the edge of the crystal. In severe cases, the crystals can be seen as fragmented.
Piece. Examples of its topography are shown in Figures 1 through 4.
4.1.1.2 Cause
When the crystal is grown or annealed, the thermal field is unreasonable, and the temperature in the furnace changes too quickly, causing thermal stress in the crystal to cause excessive cracking;
The formation of external crushing stress in the crucible causes micro-cracks at the side walls of the crystal; when seedless crystal growth occurs or there are too many impurities in the raw material, it is easy to produce localized cracks.
Polycrystalline, leading to crystal cracking.
4.1.2 Devitrification (opaque)
4.1.2.1 Morphological Features
The sapphire crystals grown are translucent or opaque and mostly blackish. An example of its topography is shown in Figure 5.
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Similar standards
How to Download GB/T 35316-2017
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 10003-2026 — Biaxially oriented polypropylene (BOPP) film
GB/T 10004-2026 — Plastic/Plastic laminated films and pouches for packaging
GB/T 10007-2026 — Rigid cellular plastics - Determination of shear properties
GB/T 35316-2017
$145.00