GB/T 33817-2017Method for determination of the carbon content on the inner surface of copper and copper-alloy tube (English PDF)
铜及铜合金管材内表面碳含量的测定方法
This is a limited preview
Buy now to download the full PDF (15 pages)
Need quotation for your management?
Get a formal quotation for GB/T 33817-2017 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
May 31, 2017
Implementation date
December 1, 2017
Scope
GB/T 33817-2017 is the English-translated version of 铜及铜合金管材内表面碳含量的测定方法.
GB/T 33817-2017 is the Chinese test method for the carbon left in or on the inner surface of copper and copper-alloy tube, over a range of 5 mg/m² to 500 mg/m².
The tube sample is burnt in an oxygen stream and the carbon dioxide produced is measured by infrared absorption in a tube-furnace carbon and sulfur analyser, giving residual carbon and total carbon, with potential carbon obtained as the difference.
It defines those three quantities, lists the reagents - 99.99% oxygen, carbon-dioxide-free water, tetrachloroethylene, trichloroethylene, trichloroethane, diluted nitric acid, two mannitol standard solutions, soda asbestos and anhydrous magnesium perchlorate - and sets out specimen preparation, the furnace at 600 °C ± 10 °C, duplicate measurements, blank and calibration tests, the calculation, the precision and the test report. Issued on 31 May 2017, it has applied since 1 December 2017.
Found what you need?
Document preview — GB/T 33817-2017
National Standard of the People's Republic of China
- ICS
- 77.120.99
- Classification
- H 13
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- Foreword3
- 1 Scope4
- 2 Terms and Definitions4
- 3 Method Summary4
- 4 Reagents5
- 5 Apparatus5
- 6 Specimen6
- 7 Test Procedures9
- 8 Calculation of Analysis Results10
- 9 Precision11
- 10 Test Report12
- Appendix A (Informative) Recommended Analysis Condition13
Foreword
This Standard was drafted as per the rules specified in GB/T 1.1-2009.
1 Scope
This Standard specifies the method for determination of carbon content in copper and copper-alloy tube or on the inner surface of tube.
This Standard is applicable to the quantitative test of carbon content in n copper and copper-alloy tube or on the inner surface of tube; the measuring range is 5mg/m² ~ 500mg/m².
2 Terms and Definitions
The following terms and definitions are applicable to this document.
2.1 Residual carbon (CR)
The carbon existing in the single substance form.
2.2 Potential carbon (CP)
The carbon existing in the organic compounds (e.g.. organic compounds of oil, grease, etc.).
2.3 Total carbon (CT)
The total sum of residual carbon and potential carbon.
3 Method Summary
Heat the copper and copper-alloy tube or tube sample in the oxygen stream to certain temperature, and burn the carbon existing on the inner surface. Use the infrared absorption spectroscopy to determine the generated carbon dioxide; then measure the content of residual carbon and potential carbon, respectively.
The content of potential carbon shall be calculated by substracting the residual carbon from total carbon.
4 Reagents
4.1 Oxygen (minimum mass purity of 99.99%). the oxygen that can be purified to 99.99% by the purifier.
4.2 Deionized water (containing no carbon dioxide). boil the deionized water for 30min; inject the oxygen (4.1) for 15min during the process of cooling off the deionized water to the room temperature; prepare before use.
4.3 Tetrachloroethylene (analytically pure).
4.4 Trichloroethylene (analytically pure).
4.5 Trichloroethane (analytically pure).
4.6 Nitric acid (1+1).
4.7 Mannitol Standard Solution A. weigh 1.2640g of mannitol (C6H14O6, pre-dry at 100°C~105°C, and place into the desiccator to cool off to the room temperature); place into 100mL beaker; add deionized water (4.2) to dissolve. Transfer into 100mL volumetric flask; dilute with deionized water (4.2) to the scale; mix evenly. 1µL of such solution contains 5µg of carbon.
4.8 Mannitol Standard Solution B. transfer 10.00mL of mannitol standard solution (4.7) into 100mL volumetric flask; dilute with deionized water (4.2) to the scale; mix evenly. 1µL of such solution contains 5µg of carbon.
4.9 Carbon dioxide gas (minimum mass purity of 99.99%).
4.10 Soda asbestos.
4.11 Anhydrous magnesium perchlorate.
5 Apparatus
5.1 Tube furnace heating-infrared carbon and sulfur analyzer
The connection schematic diagram of the device can refer to Figure 1. The burning process is implemented in the quartz pipe.
6 Specimen
6.3.3 Use the cleaning square saws or bow saws with dense teeth to cut off the required length; avoid the overheating of the specimen.
6.3.4 If the specimen length is greater than the length of combustion zone specified by the combustion device in the sample chamber; cut the pipe fitting into two parts; so that the two parts can enter into the combustion zone at the same time. If using the electric saws, ensure the all saw surfaces contacting with the pipe fitting surface have been degreased. When cutting and filing the pipe fitting, ensure the pipe sample is fixed firmly (for instance, placing into the pliers) without excessive distortion.
6.3.5 When the diameter of copper and copper-alloy tube or pipe fitting exceeds the furnace diameter, flatten the copper and copper-alloy tube and pipe fitting, so that obtain the specimen with the inner surface meeting the requirements of test.
7 Test Procedures
7.1 Specimen
Take the prepared specimen (see 6.3).
7.2 The number of measurement
Perform two separate measurements, then take their average value.
7.3 Preparation before analysis
Inject the oxygen, check whether the pipe and piston of the whole device leaks gas.
Adjust and maintain the instrument into the normal working state. Turn on the power and raise temperature to 600°C±10°C. The recommended analysis condition can refer to Appendix A.
7.4 Blank test
7.4.1 Perform two blank tests before measurement
7.4.2 Take the blank test specimen (see 6.2.4, 6.3); measure as per 7.6; the blank value shall be calculated by the total surface area (inner and outer surface areas) of the blank specimen. The blank value shall be the arithmetic mean of two specimens measured; the blank value shall be no greater than 1.5mg/m².
7.4.3 If the blank value is too large, the specimen preparation shall be re-evaluated and re-set the blank value.
7.5 Calibration test
7.5.1 According to the carbon content in the specimen, select the corresponding […]
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Referenced standards
Similar standards
How to Download GB/T 33817-2017
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 10003-2026 — Biaxially oriented polypropylene (BOPP) film
GB/T 10004-2026 — Plastic/Plastic laminated films and pouches for packaging
GB/T 10007-2026 — Rigid cellular plastics - Determination of shear properties
GB/T 33817-2017
$125.00