GB/T 29852-2013Test method for measuring Phosphorus, Arsenic and Antimony in silicon materials used for photovoltaic applications by secondary ion mass spectrometry (English PDF)
光伏电池用硅材料中P、As、Sb施主杂质含量的二次离子质谱测量方法
This is a limited preview
Buy now to download the full PDF (15 pages)
Need quotation for your management?
Get a formal quotation for GB/T 29852-2013 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
November 12, 2013
Implementation date
April 15, 2014
Scope
GB/T 29852-2013 is the English-translated version of 光伏电池用硅材料中P、As、Sb施主杂质含量的二次离子质谱测量方法.
GB/T 29852-2013 is the Chinese standard "Test method for measuring Phosphorus, Arsenic and Antimony in silicon materials used for photovoltaic applications by secondary ion mass spectrometry".
Its scope clause reads: This standard specifies the method for the determination of photovoltaic cells with secondary ion mass spectrometry (SIMS) with silicon phosphorus, arsenic and antimony content.
This standard applies to solar cell silicon material donor impurity phosphorus, arsenic and antimony content quantitative analysis in which phosphorus, arsenic and antimony concentrations were Greater than 1 × 1014atoms/cm3.
Its clauses include principle of the method; disturbances; instruments and equipment.
Found what you need?
Document preview — GB/T 29852-2013
National Standard of the People's Republic of China
- ICS
- 29.045
- Classification
- H 82
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- 1 Scope
- 2 principle of the method
- 3 disturbances
- 4 instruments and equipment
1 Scope
This standard specifies the method for the determination of photovoltaic cells with secondary ion mass spectrometry (SIMS) with silicon phosphorus, arsenic and antimony content.
This standard applies to solar cell silicon material donor impurity phosphorus, arsenic and antimony content quantitative analysis in which phosphorus, arsenic and antimony concentrations were
Greater than 1 × 1014atoms/cm3.
2 principle of the method
Under high vacuum, a cesium ion source generating primary ions, the accelerated, purified and focused, bombarding the sample surface, a variety of sputtered particle
Son, in which ions (ie, secondary ion) leads, by a different charge to mass ratio mass spectrometer to separate ions, record and calculate the sample of phosphorus, arsenic,
Secondary ion intensity ratio of antimony and silicon (31P -)/(30Si -), (75As -)/(30Si -), (121Sb -)/(30Si-), and then by using the relative sensitivity
Child quantified.
3 disturbances
3.1
sample surface adsorption of phosphorus, arsenic, antimony interfere with the sample of phosphorus, arsenic, antimony measurements.
3.2
from SIMS instrument sample chamber adsorbed to the surface of the sample can interfere with boron and aluminum samples of phosphorus, arsenic, antimony measurements.
3.3
in the sample holder window range of the sample surface should be flat, in order to ensure that each sample is moved to the analysis position, its surface with an ion collector
The inclination of the optical system unchanged, otherwise the measurement accuracy and precision will be reduced.
3.4
Measuring accuracy and precision with the sample surface roughness increases significantly reduced, the surface of the sample by chemical mechanical polishing
Light be eliminated.
3.5
Standard samples of phosphorus, arsenic, antimony uneven distribution will affect the measurement accuracy.
3.6
Standard samples of phosphorus, arsenic, antimony nominal concentration variation causes a measurement bias.
3.7
due to different instruments or different instruments in the same state, the detection limit may be different.
3.8
Because the secondary ion mass spectrometry is a destructive test, it should be sampled and the samples taken shall be representative of the nature of the batch of silicon materials.
This standard does not establish uniform methods of sampling, as most appropriate sampling plan based on different samples circumstances are different. In order to achieve secondary
Conference purpose, the sampling plan should be tested before the test to get the two sides recognized.
4 instruments and equipment
4.1 magnetic sector SIMS
Instruments need to equip a cesium ion source, capable of detecting the negative ion secondary electron multiplier and a Faraday cup detector, mass resolution better than 4000.
4.2 cryogenic liquid nitrogen or liquid helium cooling plates
If the vacuum analysis chamber is greater than 1.3 × 10-6Pa, application of liquid nitrogen or liquid helium cryogenic cooling plate surround analysis chamber sample holder.
If the vacuum analysis chamber is less than 1.3 × 10-6Pa, the cooling is not required.
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Similar standards
How to Download GB/T 29852-2013
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 10003-2026 — Biaxially oriented polypropylene (BOPP) film
GB/T 10004-2026 — Plastic/Plastic laminated films and pouches for packaging
GB/T 10007-2026 — Rigid cellular plastics - Determination of shear properties
GB/T 29852-2013
$95.00