GB/T 40913-2021Method for the determination of the hot-end coating thickness of glass bottle (English PDF)
玻璃瓶罐热端涂层厚度的测定方法
This is a limited preview
Buy now to download the full PDF (15 pages)
Need quotation for your management?
Get a formal quotation for GB/T 40913-2021 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
November 26, 2021
Implementation date
June 1, 2022
Scope
GB/T 40913-2021 is the English-translated version of 玻璃瓶罐热端涂层厚度的测定方法.
GB/T 40913-2021 sets out how to measure the thickness of the tin oxide hot-end coating on glass bottles, from 0 Å to 99 Å on the mouth and body. The light reflected by the coated surface depends on the angle of incidence, the refractive index and the coating thickness, so the thickness is measured from the reflected light.
The document specifies an induction fluid with a refractive index close to that of glass, uncoated calibration samples and samples of known thickness (17 Å to 35 Å), and an instrument accurate to 2 Å with a rotating test table.
It also sets sample conditions, such as a glass thickness of at least 1.1 mm at the measured point, and covers the procedure, data processing and test report. It was issued on 26 November 2021 and has applied since 1 June 2022.
Found what you need?
Document preview — GB/T 40913-2021
National Standard of the People's Republic of China
- ICS
- 81.040.01
- Classification
- Y 22
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- Foreword3
- 1 Scope4
- 2 Normative references4
- 3 Terms and definitions4
- 4 Principle4
- 5 Reagents or materials5
- 6 Apparatus5
- 7 Sample5
- 8 Test procedure5
- 9 Test data processing6
- 10 Test report6
1 Scope
This document describes a method for the determination of the hot-end coating thickness of glass bottle tin oxide.
This document applies the determination of the hot-end coating thickness in the range of 0 Å ~ 99 Å on the mouth and bottle body of various glass bottles.
2 Normative references
The following documents, in whole or in part, are normatively referenced in this document and are indispensable for its application. For dated references, only the version corresponding to that date is applicable to this document; for undated references, the latest version (including all amendments) is applicable to this document.
GB/T 8170, Rules of rounding off for numerical values & expression and judgment of limiting values
3 Terms and definitions
The following terms and definitions are applicable to this document.
3.1 Hot-end coating
A layer of tin oxide coating formed by the decomposition of the spray material on the hot outer surface of the glass (400 °C ~ 600 °C).
4 Principle
After the hot-end spraying of glass bottles, a tin oxide coating shall be formed on the outer surface of the glass. The amount of light reflected on the surface of the glass with tin oxide is related to the incident angle, refractive index and thickness of the tin oxide material. Where the incident angle and refractive index are known, the thickness of the tin oxide coating can be measured by the amount of reflected light.
5 Reagents or materials
5.1 Induction fluid
The refractive index is close to the refractive index of conventional glass nD20 = 1.5 (Sodium lamp D line with wavelength of 5 893 × 10^-10 m); there shall be no bubbles; it should be stored in the dark and avoid humid environment.
5.2 Calibration samples
5.2.1 Standard parts without hot-end spraying (0 Å).
5.2.2 Standard parts with known hot-end spraying thickness (17 Å ~ 35 Å).
Note: Å is the unit of measurement data of the hot-end coating thickness of glass bottles. The glass industry at home and abroad usually adopts CTU (coating thickness unit), 1 CTU ~ 1 Å (10^-10 m).
6 Apparatus
6.1 Hot-end coating thickness measuring equipment, with an accuracy of 2 Å.
6.2 The equipment shall include a testing table that can fix glass bottles, and the testing table shall be able to rotate manually or automatically.
7 Sample
7.1 The thickness of the glass at the measured position of the sample shall not be less than 1.1 mm.
7.2 The measured position of the sample shall be free from defects such as stains and bubbles.
7.3 The sample shall be annealed normally, cooled to room temperature, and kept dry.
8 Test procedure
8.1 Turn on the hot-end coating thickness measuring instrument; check the induction liquid pipe, and confirm that there are no air bubbles. Use calibration samples to check the measurement accuracy of the instrument after the equipment is turned on the day of use.
8.2 Put the sample on the testing table and adjust the measuring probe to the target height. […]
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Referenced standards
Similar standards
How to Download GB/T 40913-2021
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 8170-1987 — Rules for rounding off of numerical values