Valid

GB/T 38596-2020Determination method of heavy metal contents in the wastewater during catalyst production (English PDF)

催化剂生产废水中重金属含量的测定

Preview PDF

This is a limited preview

Buy now to download the full PDF (15 pages)

Need quotation for your management?

Get a formal quotation for GB/T 38596-2020 in 30 minutes.

Issued by

SAMR; SAC

Level / Type

National · Recommended

Issue date

March 31, 2020

Implementation date

February 1, 2021

Scope

GB/T 38596-2020 is the English-translated version of 催化剂生产废水中重金属含量的测定.

GB/T 38596-2020 is the Chinese standard "Determination method of heavy metal contents in the wastewater during catalyst production". Its scope clause reads: This standard specifies the determination method of heavy metal content in catalyst production wastewater.

This standard applies to the total amount and dissolution of copper (Cu), lead (Pb), bismuth (Bi), antimony (Sb), cobalt (Co), and nickel (Ni) in catalyst production wastewater Determination of state content. Its clauses include general rules; reagents or materials; samples.

Found what you need?

Document preview — GB/T 38596-2020

National Standard of the People's Republic of China

ICS
71.100.99
Classification
G 74

Issued by: State Administration for Market Regulation; Standardization Administration of the PRC

Contents

  • 1 Scope
  • 2 Normative references
  • 3 General rules
  • 4 Reagents or materials
  • 5 samples

1 Scope

This standard specifies the determination method of heavy metal content in catalyst production wastewater.

This standard applies to the total amount and dissolution of copper (Cu), lead (Pb), bismuth (Bi), antimony (Sb), cobalt (Co), and nickel (Ni) in catalyst production wastewater

Determination of state content.

2 Normative references

The following documents are indispensable for the application of this document. For dated reference documents, only the dated version applies to this article

Pieces. For undated references, the latest version (including all amendments) applies to this document.

GB/T 602 Preparation of standard solutions for impurity determination of chemical reagents

Preparation of preparations and products used in GB/T 603 chemical reagent test method

GB/T 6682 Analytical laboratory water specifications and test methods

3 General rules

When there are no other requirements for the reagents used in this standard, inductively coupled plasma emission spectroscopy uses superior grade pure reagents, flame atoms

Absorption spectroscopy uses analytical reagents; when no other requirements are specified, the water used refers to the secondary water specified in GB/T 6682.Testing

The standard solutions, preparations and products used for impurity determination are in accordance with the regulations of GB/T 602 and GB/T 603 unless other requirements are specified.

Order preparation.

4 Reagents or materials

4.1

Nitric acid.

4.2

Perchloric acid.

4.3 Nitric acid solution

11.

4.4 Nitric acid solution

99.

4.5 Copper standard solution

1g/L. Weigh 1g (accurate to 0.0001g) of metallic copper (spectral purity), and heat it with 30mL nitric acid solution (4.3) to dissolve it.

After cooling, make the volume to 1L with water.

4.6 Lead standard solution

1g/L. Weigh 1g (accurate to 0.0001g) of metallic lead (spectral purity), and heat it with 30mL nitric acid solution (4.3) to dissolve it.

After cooling, make the volume to 1L with water.

4.7 Bismuth standard solution

1g/L. Weigh 1g (accurate to 0.0001g) of metallic bismuth (spectral purity), and use 50mL of nitric acid solution (4.3) to heat it to dissolve

After dissolving completely, cool to room temperature and dilute to 1L with water.

4.8 Antimony standard solution

1g/L. Weigh 1g (accurate to 0.0001g) metal antimony (spectral purity), and use 20mL~30mL sulfuric acid solution (1 1) Heat to dissolve, and dilute to 1L with sulfuric acid solution (1 4).

4.9 Cobalt standard solution

1g/L. Weigh 1g (accurate to 0.0001g) of metallic cobalt (spectrally pure), and use 50mL of nitric acid solution (4.3) to heat to dissolve

After cooling, make the volume to 1L with water.

4.10 Nickel standard solution

1g/L. Weigh 1g (accurate to 0.0001g) of metallic nickel (spectral purity) and heat it with 30mL nitric acid solution (4.3)

Dissolve and dilute to 1L with water after cooling.

4.11

Copper, lead, bismuth, antimony, cobalt, and nickel mixed standard solutions. copper, lead, bismuth, antimony, cobalt, and nickel are all 100 mg/L. Measure 10.00mL copper separately

Standard solution (4.5), lead standard solution (4.6), bismuth standard solution (4.7), antimony standard solution (4.8), cobalt standard solution (4.9), nickel standard solution (4.10) Placed in a 100mL volumetric flask, add 4mL of nitric acid solution (4.3), dilute to 100mL with water, and shake well.

4.12 Copper, lead, and nickel mixed standard solution

copper, lead, and nickel are all 100mg/L. Measure 10.00mL copper standard solution as needed (4.5) One or more of lead standard solution (4.6) and nickel standard solution (4.10) are placed in a 100mL volumetric flask, and 5mL nitric acid solution is added (4.3), dilute to 100mL with water, shake well.

5 samples

5.1 Collect samples with polyethylene bottles

The sampling bottle is first washed with detergent, then soaked in nitric acid solution (4.3), and rinsed with water before use clean.

5.2

Analyze the sample of the total amount of elements, add appropriate amount of nitric acid immediately after collection to make the volume fraction of nitric acid reach 1%. Measure 10.00mL after acidification

In a 100mL beaker, add 5.0mL nitric acid solution (4.3) and cover with a watch glass. Place it on the hot plate and put it in a near boiling state

The sample evaporates to nearly dryness. After cooling, repeat the above operation once, adding nitric acid or perchloric acid if necessary, until the dissolution is complete. After steaming until nearly dry,

Remove to cool. Add water to dissolve the residue. If there is any insoluble precipitate, filter through quantitative filter paper, transfer to a 100mL volumetric flask, and add nitric acid solution (4.4) Constant volume, shake well, to be tested.

5.3

When analyzing a sample with dissolved element content, the sample is immediately filtered through a 0.45µm filter membrane after collection, and the obtained filtrate is immediately added to the appropriate amount

Nitric acid, so that the nitric acid content reaches 1%. Measure 10.00mL of acidified sample into a 100mL volumetric flask, and dilute to volume with nitric acid solution (4.4)

To 100mL, shake well, to be tested.

6 Determination of copper, lead, bismuth, antimony, cobalt, and nickel content---inductively coupled plasma atomic emission spectrometry

6.1 Principle

The filtered or digested sample is injected into the inductively coupled plasma emission spectrometer, and the carrier gas is carried into the plasma, and the excited atoms

And ion emits atomic spectrum and ion spectrum, and its content is measured by the intensity of element characteristic spectrum.

6.2 Instruments

6.2.1

Inductively coupled plasma atomic emission spectrometer.

6.2.2

The electric heating plate can be adjusted.

6.3 Test procedure

6.3.1 Drawing of working curve

Take six 100mL volumetric flasks, add copper, lead, bismuth, antimony, cobalt, nickel mixed standard solution (4.11) 0mL, 1.00mL,

2.00mL, 3.00mL, 4.00mL, 5.00mL, dilute to 100mL with nitric acid solution (4.4), shake well. According to the optimal working conditions of the instrument,

Use a high-purity argon plasma torch at the recommended wavelengths of 324.75nm (copper), 220.35nm (lead), 223.06nm (bismuth), 206.83nm (Antimony), 228.62nm (cobalt), 231.60nm (nickel) of the analytical line signal intensity of the solution. Based on the mass concentration of the element to be measured in the above solution

Degree (mg/L) is the abscissa, the signal intensity of the analysis line of the element to be measured is the ordinate, and the working curve is drawn.

6.3.2 Determination

On the inductively coupled plasma atomic emission spectrometer, the sample solution was measured under the same conditions as the standard solution series (5.2, 5.3) and the blank solution (take the same volume of water as the sample to prepare the blank solution according to the provisions of 5.2 and 5.3) analysis line signal intensity, from

Find the corresponding mass concentration on the working curve. During the sample determination process, if the mass concentration of the element to be tested in the sample exceeds the working curve range, the sample

Need to re-measure after dilution.

6.4 Test data processing

The total amount of the element to be measured or the dissolved mass concentration rho, the value is expressed in milligrams per liter (mg/L), calculated according to formula (1).

Take the arithmetic average of two parallel determination results as the determination result.

The absolute difference between two independent test results obtained under repeatability conditions should not be greater than 10% of the arithmetic mean.

6.5 Detection limit

The detection limits of various elements are shown in Table 1.

7.1 Principle

The filtered or digested sample is introduced into the air-acetylene flame of the atomic absorption spectrometer, and the absorbance of each element to be measured is measured, and

Compare and quantify the absorbance with the corresponding element working curve.

7.2 Equipment

7.2.1 Atomic absorption spectrometer

equipped with flame atomizer, with copper, lead, nickel hollow cathode lamp.

7.2.2

The electric heating plate can be adjusted.

7.3 Test procedure

7.3.1 Drawing of working curve

Take six 100mL volumetric flasks, add copper, lead, nickel mixed standard solution (4.12) 0mL, 1.00mL, 2.00mL, 3.00mL,

4.00mL, 5.00mL, dilute to 100mL with nitric acid solution (4.4), shake well. On the atomic absorption spectrometer, press the optimal working bar of the instrument

Set to zero with a blank solution without standard solution, and in the order of mass concentration from low to high, the recommended wavelength is 324.8nm,

Measure the absorbance of copper, lead and nickel at 217.0nm and 232.0nm. Take the mass concentration (mg/L) of copper, lead, and nickel in the above solution as horizontal

The coordinate, the corresponding absorbance value is the ordinate, and the working curve is drawn.

7.3.2 Determination

On the atomic absorption spectrometer, the sample solution (5.2, 5.3) and the blank solution were measured under the same conditions as the standard solution series.

The absorbance of the liquid (take the same volume of water as the sample to prepare a blank solution according to the provisions of 5.2 and 5.3), and find the corresponding mass concentration from the working curve degree. In the process of sample determination, if the mass concentration of the element to be tested in the sample exceeds the range of the working curve, the sample needs to be diluted and re-measured.

7.4 Test data processing

The total amount of the measured element or the dissolved mass concentration rho2, the value is expressed in milligrams per liter (mg/L), calculated according to formula (2).

Take the arithmetic average of two parallel determination results as the determination result.

The absolute difference between two independent test results obtained under repeatability conditions should not be greater than 10% of the arithmetic mean.

7.5 Detection limit

The detection limits of various elements are shown in Table 2.

......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.

Similar standards

How to Download GB/T 38596-2020

  1. 1

    Add to cart

    Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.

  2. 2

    Checkout

    Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).

  3. 3

    Fast delivery

    After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.

  4. 4

    Invoice included

    A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.

Related Standards

English PDF
15 pages
Fast delivery
Invoice included
View Cart

Secure payment via Stripe

Payments accepted

VisaMastercardAmerican ExpressApple PayGoogle PayStripe

GB/T 38596-2020

$85.00