Valid

GB/T 26492.5-2011Defects of wrought aluminium and aluminium alloys ingots and products - Part 5: Defects for tubes,rods or bars,profiles,wires (English PDF)

变形铝及铝合金铸锭及加工产品缺陷 第5部分:管材、棒材、型材、线材缺陷

Preview PDF

This is a limited preview

Buy now to download the full PDF (17 pages)

Need quotation for your management?

Get a formal quotation for GB/T 26492.5-2011 in 30 minutes.

Issued by

SAMR; SAC

Level / Type

National · Recommended

Issue date

May 12, 2011

Implementation date

February 1, 2012

Scope

GB/T 26492.5-2011 is the English-translated version of 变形铝及铝合金铸锭及加工产品缺陷 第5部分:管材、棒材、型材、线材缺陷.

GB/T 26492.5-2011 is the Chinese standard "Defects of wrought aluminium and aluminium alloys ingots and products - Part 5: Defects for tubes,rods or bars,profiles,wires".

Its scope clause reads: This section provides aluminum and aluminum alloy tubes, definitions rods, profiles and wire products, common defects, features, and analyzes its main production Health reasons.

This section applies to the determination and analysis of aluminum and aluminum alloy tubes, rods, profiles, wire defects. Its clauses include definition of defects, features and main causes.

Found what you need?

Document preview — GB/T 26492.5-2011

National Standard of the People's Republic of China

ICS
77.150.10
Classification
H 60

Issued by: State Administration for Market Regulation; Standardization Administration of the PRC

Contents

  • 1 Scope
  • 2 Definition of Defects, features and main causes
  • 2.1 Bubble blister
  • 2.2 From the skin peeling

1 Scope

This section provides aluminum and aluminum alloy tubes, definitions rods, profiles and wire products, common defects, features, and analyzes its main production

Health reasons.

This section applies to the determination and analysis of aluminum and aluminum alloy tubes, rods, profiles, wire defects.

2 Definition of Defects, features and main causes

2.1 Bubble blister

Continuous or discontinuous raised bubbly cavity surface of the article (Figure 1).

The main causes.

a) Extrusion or extrusion pad water, oil and dirt;

b) the air enters the metal surface during extrusion;

c) lubricants in water;

d) There ingot loose, porosity;

e) product hydrogen content is too high;

f) Extrusion temperature and the ingot temperature is too high.

Figure 1 Bubble

2.2 From the skin peeling

A thin layer on the surface of the article is attached, there are local peeling (Figure 2).

The main causes.

a) extrusion cylinder is not clean;

b) extrusion cylinder and pressure pads mismatch;

c) a metal stick with a long work on mold or die orifice.

Figure 2 from the skin […]

......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 17 pages — is available in the English PDF.

Referenced standards

Similar standards

How to Download GB/T 26492.5-2011

  1. 1

    Add to cart

    Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.

  2. 2

    Checkout

    Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).

  3. 3

    Instant delivery (0–9 sec)

    Delivery is automatic: within seconds of payment you'll receive an email with a secure download link. The link stays valid for 72 hours.

  4. 4

    Invoice included

    A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.

Related Standards

English PDF
17 pages
Instant delivery (0–9 sec)
Invoice included
View Cart

Secure payment via Stripe

Payments accepted

VisaMastercardAmerican ExpressApple PayGoogle PayStripe

GB/T 26492.5-2011

$295.00