Valid

YS/T 745.3-2010Methods for chemical analysis of copper anode slime. Part 3: Determination of platinum content and palladium comtent. Fire assay collection-inductively coupled coupled plasma atomic emission spectrometric methods (English PDF)

铜阳极泥化学分析方法 第3部分:铂量和钯量的测定火试金富集-电感耦合等离子体发射光谱法

Preview PDF

This is a limited preview

Buy now to download the full PDF (4 pages)

Need quotation for your management?

Get a formal quotation for YS/T 745.3-2010 in 30 minutes.

Issued by

Ministry of Industry and Information Technology

Level / Type

National · Recommended

Issue date

November 22, 2010

Implementation date

March 1, 2011

Scope

YS/T 745.3-2010 is the English-translated version of 铜阳极泥化学分析方法 第3部分:铂量和钯量的测定火试金富集-电感耦合等离子体发射光谱法.

YS/T 745.3-2010 — YS/T 745 This section specifies the determination of copper anode slime platinum and palladium content. This section applies to the determination of platinum, palladium, copper anode mud content. Measuring range Pt 5.00g/t ~ 100.00g/t; palladium 10.00g/t ~ 150.00g/t.

Found what you need?

Document preview — YS/T 745.3-2010

National Standard of the People's Republic of China

ICS
77.120.01
Classification
H 14

Issued by: Ministry of Industry and Information Technology

Contents

  • Foreword
  • 1 Scope
  • 2 Method summary
  • 3 Reagents

Foreword

YS/T 745 "Methods for chemical analysis of copper anode mud" is divided into nine sections.

--- Part 1. Determination of copper content iodometry;

--- Part 2. gold and silver content determination fire assay gravimetric method;

--- Part 3. the amount of platinum and palladium contents - fire assay enrichment - Inductively coupled plasma atomic emission spectrometry;

--- Part 4. Determination of the amount of selenium iodometry;

--- Part 5. Determination of tellurium content dichromate method;

--- Part 6. Determination of lead content Na2EDTA titration;

--- Part 7. Determination of bismuth content - Flame atomic absorption spectrometric method and Na2EDTA titration;

--- Part 8. Determination of arsenic content by hydride generation - atomic fluorescence spectrometry;

--- Part 9. Determination of antimony content - Flame atomic absorption spectrometry.

This is Part 3.

This section is in accordance with GB/T 1.1-2009 given rules drafted.

The non-ferrous metal part by the National Standardization Technical Committee (SAC/TC243) centralized.

This section is responsible for drafting unit. Daye Nonferrous Metals Corporation.

This section is drafted. Beijing General Research Institute of Mining and Metallurgy.

Participated in the drafting of this section. Daye Nonferrous Metals Corporation, Tongling Nonferrous Metals Group Holdings Co., Jiangxi Copper shares have Ltd., Jinchuan Group Limited, Northern Copper Co., Ltd., Guangzhou Nonferrous Metal Research Institute, Hunan Nonferrous Metals Research Institute.

1 Scope

YS/T 745 This section specifies the determination of copper anode slime platinum and palladium content.

This section applies to the determination of platinum, palladium, copper anode mud content. Measuring range Pt 5.00g/t ~ 100.00g/t; palladium 10.00g/t ~ 150.00g/t.

2 Method summary

Sample by fire assay enrichment, the formation of co-grain containing platinum palladium. After co-grain mixed acid dissolution, by inductively coupled plasma atomic emission spectrometry Instrument Determination solution of platinum and palladium.

3 Reagents

Unless otherwise indicated in the analysis using only recognized as analytical grade reagents and distilled or deionized water or equivalent purity.

3.1 anhydrous sodium carbonate, commercially pure.

3.2 Lead oxide, palladium-platinum-free, commercially pure.

3.3 silica, commercially pure.

3.4 borax, commercially pure.

3.5 sodium chloride, commercially pure.

3.6 starch.

3.7 nitric acid (17), no chlorine ions.

3.8 glacial acetic acid (13).

3.9 mixed acid. hydrochloric acid, nitric acid (31), (now with the current).

3.10 platinum standard stock solution. Weigh 0.1000g platinum (>=99.9%) in 100mL beaker, add 20mL mixed acid (3.9), plus After dissolving heat, add 5 drops of sodium chloride solution 200g L /, on the steam bath to nearly dry, add 20mL hydrochloric acid dissolved and transferred to 100mL volumetric flask the diluted with water to volume, and mix. 1mL solution containing 1mg platinum.

3.11 palladium standard stock solution. Weigh 0.1000g of palladium (>=99.9%) in 100mL beaker 20mL mixed acid (3.9), heating After dissolution, add 5 drops of sodium chloride solution 200g L /, on the steam bath to nearly dry, add 20mL dissolved in hydrochloric acid and transferred to 100mL volumetric flask the diluted with water to volume, and mix. 1mL solution containing 1mg palladium.

3.12 platinum, palladium mixed standard solution. platinum were taken above the standard stock solution (3.10), palladium standard stock solution (3.11) each 10.00mL in 100mL flask, add 10mL mixed acid (3.9), diluted with water to volume, and mix. This solution 1mL containing 100µg platinum, 100µg palladium.

......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 4 pages — is available in the English PDF.

Referenced standards

How to Download YS/T 745.3-2010

  1. 1

    Add to cart

    Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.

  2. 2

    Checkout

    Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).

  3. 3

    Instant delivery (0–9 sec)

    Delivery is automatic: within seconds of payment you'll receive an email with a secure download link. The link stays valid for 72 hours.

  4. 4

    Invoice included

    A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.

Related Standards

English PDF
4 pages
Instant delivery (0–9 sec)
Invoice included
View Cart

Secure payment via Stripe

Payments accepted

VisaMastercardAmerican ExpressApple PayGoogle PayStripe

YS/T 745.3-2010

$115.00