GB/T 37829-2019Iron ore fines in bulk—Determination of transportable moisture limits—Flow-table method (English PDF)
散装铁矿粉 适运水分限量的测定 流盘试验法
This is a limited preview
Buy now to download the full PDF (15 pages)
Need quotation for your management?
Get a formal quotation for GB/T 37829-2019 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
August 30, 2019
Implementation date
July 1, 2020
Scope
GB/T 37829-2019 is the English-translated version of 散装铁矿粉 适运水分限量的测定 流盘试验法.
GB/T 37829-2019 is the Chinese standard "Iron ore fines in bulk—Determination of transportable moisture limits—Flow-table method". Its scope clause reads: This Standard specifies the flow-table test method for the transportable moisture limit (TML) of iron ore fines in bulk.
This Standard is applicable to the determination of the transportable moisture limit of iron ore fines with a nominal maximum particle size of 1 mm; and iron ore fines with a nominal maximum particle size of 1 mm ~ 7 mm can be used as a reference.
Its clauses include preparation of the specimen; main test of flow moisture point; precision; test report.
Found what you need?
Document preview — GB/T 37829-2019
National Standard of the People's Republic of China
- ICS
- 73.060.10
- Classification
- D 31
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- Foreword3
- 1 Scope4
- 2 Normative References4
- 3 Terms and Definitions5
- 4 Principle5
- 5 Instrument5
- 6 Preparation of the Specimen6
- 7 Pre-Test of Flow Moisture Point7
- 8 Main Test of Flow Moisture Point8
- 9 Calculation of Flow Moisture Point9
- 10 Calculation of Transportable Moisture Limits (TML)9
- 11 Precision10
- 12 Test Report10
- Appendix A (Normative) Flow Table Instrument and Rammer11
- Appendix B (Informative) Specimen for Precision Test17
1 Scope
This Standard specifies the flow-table test method for the transportable moisture limit (TML) of iron ore fines in bulk.
This Standard is applicable to the determination of the transportable moisture limit of iron ore fines with a nominal maximum particle size of 1 mm; and iron ore fines with a nominal maximum particle size of 1 mm ~ 7 mm can be used as a reference.
2 Normative References
The following documents are essential to the application of this document. For the dated documents, only the versions with the dates indicated are applicable to this document; for the undated documents, only the latest version (including all the amendments) is applicable to this document.
GB/T 6379.1 Accuracy (Trueness and Precision) of Measurement Methods and
Results - Part 1: General Principles and Definitions
GB/T 6379.2 Accuracy (Trueness and Precision) of Measurement Methods and
Results - Part 2: Basic Method for the Determination of Repeatability and
Reproducibility of a Standard Measurement Method
GB/T 10322.1 Iron Ores - Sampling and Sample Preparation Procedures
GB/T 10322.5 Iron Ores - Determination of the Moisture Content of a Lot
GB/T 20565 Iron Ores and Direct Reduced Iron - Vocabulary […]
5.4 Measuring cylinder
A glass measuring cylinder with a scale of 100mL and 10mL
respectively.
5.5 Mixing container
A mixing container capable of satisfying about 5kg of iron ore fines or an automatic mixer of a considerable size.
5.6 Balance
The maximum weighable is no less than 2kg, accurate to 0.1g.
5.7 Oven
With automatic temperature control and blast device, the temperature can be controlled at 105°C±5°C.
5.8
Vernier calliper, accurate to 0.1mm.
6 Preparation of the Specimen
6.1 General requirements
The sample shall be carried out in a room free from changes in temperature, airflow and humidity; and the sample preparation phase and the test process shall be completed in the same day. In addition, the container for the specimen shall be a closed container or covered with plastic film and other suitable materials. In order to prevent possible changes in the fluidization characteristics of bulk iron ore fines, samples must not be broken during sample preparation.
6.2 Preparation of the specimen
Take samples according to GB/T 10322.1. Put a representative specimen of iron ore fines into a mixing container and stir thoroughly; and then divide the specimen into a specimen for original moisture measurement (Specimen A), a pre-test specimen (Specimen B) and specimens for two parallel main tests (Specimens C and D). The amount of the specimen for the original moisture measurement is about 1kg; weigh it immediately; and determine the moisture content of the specimen "on receipt" according to GB/T 10322.5. The pre-test and the single main test respectively require the specimen volume to be no less than 3 times the mould capacity. The sample volume varies with the mass ratio of iron ore fines, which is about 3kg respectively.
6.3 Filling the round mould
Place the round mould in the centre of the flow table; and fill the round mould with the specimen thoroughly stirred in the mixing container in three layers. The first layer after tamping shall account for about one-third of the depth of the round mould. The second layer after tamping shall reach about two-thirds of the depth of the round mould. And the last layer after tamping of specimen should be filled to about 5mm down from the top of the round mould.
7.2.2
The vibration of the flow table causes the particles to be re-embedded to form a
compact state, which increases the percentage of water content in the specimen in a certain state. When the moisture is saturated in the compact specimen and the specimen is plastically deformed, that is, the flow state is generated; it is considered that the moisture content of the specimen has reached the flow moisture point. At this time, the truncated cone shall deform to form a convex or concave surface. In most cases, measuring deformation helps to determine whether plastic flow has occurred.
The following states are used as one of the characteristics for judging whether the specimen has reached the plastic flow state:
a) Use a vernier calliper to measure the feature that the diameter of any part of the truncated cone increases by more than 3mm;
b) Add water equivalent to 0.4%~0.5% moisture content; repeat the procedures
6.3~6.5; vibrate the flow table for 25 times. Measure the bottom or middle diameter of the truncated cone; for the first time, the diameter shall increase by
1mm~5mm; add water again; then the bottom diameter shall increase by
5mm~10mm;
c) When the water content (increasing gradually) is close to the flow water point, the truncated cone shall have a tendency to stick in the round mould;
d) When the truncated cone is pushed out of the flow table, wet marks (streaks) shall be left on the flow table, which indicates that the water content may exceed the flow moisture point; but the invisible wet marks (streaks) do not indicate that the water content is lower than the flow moisture point.
8 Main Test of Flow Moisture Point
After reaching the fluid state in the pre-test, adjust the water content of Specimen C and Specimen D to be 1% to 2% lower than the last water content that did not cause fluidization in the pre-test. The final test is carried out by Specimen C and Specimen
D with adjusted water content. The method is the same as the pre-test, but the amount of water added each time does not exceed 0.5%. The lower the flow moisture point in the pre-test, the smaller the amount of the added water.
When the specimen taken from Specimen C and Specimen D are adjusted to start plastic flow or that of after a little water is added; the specimen in the round mould can be placed in a clean container of known mass and weighed immediately; and test the moisture content. Otherwise, put it back into the mixer container and continue with the above procedures. The moisture at this time is the that before reaching the flow state.
11 Precision
The precision data of this Standard is the test result of the joint analysis of 5 iron ore fines specimens by 10 laboratories in 2017, which is obtained by statistical analysis according to GB/T 6379.1 and GB/T 6379.2: Repeatability limit r = 0.17%, reproducibility limit R = 0.62%. Refer to Appendix B for the test specimen.
12 Test Report
The test report shall include the following contents:
a) Sample number;
b) A detailed description of the sample;
c) Basis standard (number of this Standard);
d) Special instructions;
e) Test results;
f) Any deviation from the Standard;
g) Abnormal phenomena in the test;
h) Test date.
Appendix A (Normative)
Flow Table Instrument and Rammer
A.1 Flow table instrument
A.1.1 Flow table and seat frame
The structure of the flow table is shown in Figure A.1. The flow table is composed of an integrally cast rigid iron frame and a rigid round plate with a diameter of
254mm±2.54mm; and a shaft is connected perpendicularly to the plate with a spiral thread. The plate surface connected with the shaft and the integral contact shoulder of the shaft shall be installed on a frame; so that it can be raised and dropped vertically from the specified height with a rotating cam. The allowable error of the height of the new flow table is ±0.13mm; while that of the flow table in use is ±0.39mm. The plate surface shall be a well-machined flat surface, free of bubbles or surface defects. The plate surface shall be made of brass or bronze; the Rockwell hardness number is no less than HRB25; the edge thickness is 7.62mm; and there shall be 6 integral radial strengthening ribs. The mass of the plate surface and the shaft connected to it is
4kg±0.05kg; and the mass shall be symmetrically distributed around the axis.
Unit: mm
Key:
f – line on the plate surface.
Figure A.1 – Flow Table
A.1.2 Cam and vertical shaft
The cam and vertical shaft shall be made of medium-carbon mechanical steel; and hardened at part A as shown in Figure A.2. The shaft shall be straight. The difference between the shaft diameter of the new flow table and the inner diameter of the frame cavity cylinder shall be no less than 0.05mm and no more than 0.08mm. The flow table in use shall be kept at 0.051mm~0.26mm. When the shaft falls to the end; the shaft end shall not fall on the cam; but the point of fall shall contact the cam at an angle of no less than 120°. The cam surface shall be a smooth spiral curved surface with a radius uniformly increased from 132.70mm (Translator Note: here it shall be 12.70mm according to the Figure A.2) to 31.75mm within the range of 360°; and there shall be no obvious vibration when the shaft is in contact with the cam.
The position of the cam and the contact surface between the cam and the shaft should make the rotation of the flow table no more than one revolution for 25 drops. The surface of the flow table and the frame that come into contact when falling to the bottom should remain smooth, flat and level, parallel to the upper surface of the flow table;
and continue to contact throughout the entire 360° range.
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Similar standards
How to Download GB/T 37829-2019
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 10003-2026 — Biaxially oriented polypropylene (BOPP) film
GB/T 10004-2026 — Plastic/Plastic laminated films and pouches for packaging
GB/T 10007-2026 — Rigid cellular plastics - Determination of shear properties
GB/T 37829-2019
$205.00