T/CSAE 52-2016Test method of mechanical properties for metallic sheets at high strain rates (English PDF)
金属板材在高应变速率下的力学性能测试方法——液压伺服控制系统及其他控制系统
This is a limited preview
Buy now to download the full PDF (17 pages)
Need quotation for your management?
Get a formal quotation for T/CSAE 52-2016 in 30 minutes.
Issued by
China Society of Automotive Engineers
Level / Type
National · Mandatory
Issue date
May 26, 2016
Implementation date
May 26, 2016
Scope
T/CSAE 52-2016 is the English-translated version of 金属板材在高应变速率下的力学性能测试方法——液压伺服控制系统及其他控制系统.
T/CSAE 52-2016 — This standard specifies the principles, symbols and descriptions, specimens and devices for tensile testing of automotive sheet metal at high strain rates.
This standard is applicable to automotive sheet metal with a thickness of 3mm or less (including 3mm). The strain rate required for the test is 10-2s-1~ 103s-1, test temperature is 10 ° C ~ 35 ° C (or by mutual agreement).
This standard applies to hydraulic servo test systems. Unless otherwise stated, different strain rates are selected for sheet metal of the same specification. It should be done on the same test equipment.
Note 1. When the strain rate of the test is less than 10-2s-1, the comparison test can be carried out using a quasi-static tensile tester.
Found what you need?
Document preview — T/CSAE 52-2016
National Standard of the People's Republic of China
- ICS
- 43.120
- Classification
- T 40
Issued by: China Society of Automotive Engineers
Contents
- Foreword
- Introduction
- 1 Scope
- 2 Standard References
- 3 Symbols, names and units
- 4 Principles
- 5 Test equipment
- 6 Sample
- 7 Test requirements
- 8 Test report
- Appendix A Test Equipment
- Appendix B Comparison of dynamic mechanical properties of raw materials and pre-strained
- Appendix C Test sample size
- Appendix D Engineering Stress-Engineering Strain Curve Example
- Appendix E Material dynamic mechanical properties constitutive model
- References
Foreword
According to the current mechanical and electrical test schemes for metal materials at home and abroad at high strain rates, the test equipment can be divided into two categories.
Elastic rod type system, the other type is hydraulic servo and other test systems.
This standard only applies to hydraulic servo and other servo test systems.
This standard uses the quasi-translation method to refer to ISO 26203-2:2011 "Metal material high strain rate tensile test Part 2. liquid Pressure servo and other test systems" and SEP 1230 "Mechanical properties of sheet metal at high strain rates in high-speed tensile tests determine".
The technical differences between this standard and ISO 26203-2:2011 and SEP 1230 and their reasons are as follows.
a) Regarding the scope, this standard requires that different strain rates selected for sheet metal of the same specification should be performed on the same test equipment.
To ensure comparability of test data (see Section 1);
b) Regarding the standard reference documents, the ISO /6892 is replaced by the international standard GB/T 228.1 to adapt to China.
Technical conditions (see section 2).
c) replace "this International Standard" with "this standard";
d) Replace the comma ',' as a decimal point with a decimal point '.';
e) deleted the preface to international standards;
f) In order to ensure the reliability of the test data, this standard stipulates the calibration of the test equipment;
g) Regarding the sample, make the following adjustments.
- Added calibration protocols for test equipment to ensure the reliability of test data (see Section 6.1);
- Increased processing of test samples after the material has passed the process path (see Section 6.1);
- Added instructions for testing non-plate materials or metal materials with a thickness greater than 3 mm (see Section 6.2);
- Increased the convention for sampling direction (see Section 6.3);
- Increased the number of samples required during the test (see Section 6.3);
h) Regarding data processing, due to the limited strain rate set by the test, this standard adds material constitutive model determination and gives Publish and verify the constitutive model (see Section 7.5.5);
i) Regarding the test report, make the following adjustments (see Section 8).
- Added requirements for the processing conditions and processing conditions of the sample;
- Added requirements for the location and direction of the sampling;
- Added requirements for the measurement of load and strain;
- Added requirements for the measurement of load and strain;
- Increased the number of requirements for valid data;
- Added requirements for material constitutive models and parameters;
This part is proposed by the Materials Division of the China Automotive Engineering Society.
This part is under the jurisdiction of the China Automotive Engineering Society.
This section drafted by. China Automotive Engineering Research Institute Co., Ltd.
Introduction
Many engineering materials exhibit a sensitivity to strain rate dependence, ie strain rate. To some extent, strain rate the higher the yield strength of the material, the better the energy absorption of the material. This test method is very useful for evaluating the collision of automotive structures.
important. At present, the crashworthiness of automotive structures is increasingly evaluated by numerical simulation methods, and numerical simulation can be minimized.
Cost and shortest time consumption replace traditional crash tests. What is required for numerical simulation analysis is the response of the material at high strain rates.
Force strain curve. The quasi-static value is obtained according to GB/T 228.1, that is, the strain rate is <=0.00025s-1, but this is for describing the dynamic load.
The deformation of the material of the loaded part is unsuitable, and the required strain rate under dynamic load is generally >=10-2 s-1.
T/CSAE XX-XXXX
Test method for mechanical properties of sheet metal at high strain rate
--Hydraulic servo control system and other control systems
1 Scope
This standard specifies the principles, symbols and descriptions, specimens and devices for tensile testing of automotive sheet metal at high strain rates.
This standard is applicable to automotive sheet metal with a thickness of 3mm or less (including 3mm). The strain rate required for the test is 10-2s-1~ 103s-1, test temperature is 10 ° C ~ 35 ° C (or by mutual agreement).
This standard applies to hydraulic servo test systems. Unless otherwise stated, different strain rates are selected for sheet metal of the same specification.
It should be done on the same test equipment.
Note 1. When the strain rate of the test is less than 10-2s-1, the comparison test can be carried out using a quasi-static tensile tester.
2 Standard reference documents
The following documents are indispensable for the application of this document. For dated references, only the dated version applies.
This document. For undated references, the latest edition (including all amendments) applies to this document.
GB/T 228.1-2010 tensile testing of metallic materials - Part 1 Metallic materials - High strain rate tensile test methods - Part 1 . Elastic rod systems;
ISO 26203-2. High-strength tensile test methods for metallic materials - Part 2. Hydraulic servo control and other control systems;
Determination of the mechanical properties of sheet metal at high strain rates in SEP 1230 high speed tensile test;
ASTM E 1012-2012 Standard Practice for Verifying Test Frame and Sample Alignment under Tensile and Compressive Axial Forces;
GB/T 2975 steel and steel products mechanical properties test sampling position and sample preparation.
3 Symbols, names and units
The symbols, names and units used in this standard are shown in Table 1.
Table 1 Symbols and descriptions
Symbol unit description Sample A0 mm original thickness of the sample B0 mm original width in the gauge length Bk mm width of the sample holding portion L0 mm sample original gauge length Lc mm sample parallel length Le mm extensometer gauge length T/CSAE XX-XXXX
Table 1 Symbols and descriptions (continued)
r mm The radius of the transition arc connecting the parallel section of the specimen to the clamping section Original cross-sectional area of the parallel length portion of the S0 mm2 specimen SD mm2 dynamometer area. the area of the fixed end of the sample, only the elastic deformation section is required during the test Symbol unit description time Ts time Tf s The time from the start of the test to the time the sample broke Elongation A % Elongation after break Note. The symbol A of a non-proportional sample often has a subscript, such as. A20mm indicates the original sample Elongation after breakage of gauge length L0 = 20 mm.
Elongation
Ag % Plastic elongation at maximum force Fm (plastic strain at maximum force Fm) Agg % Maximum elongation at maximum force Fm (total strain at maximum force Fm) strain e(t) % Instant engineering strain Epp % plastic engineering strain Eg % total engineering strain Epp -- plastic true strain Eg -- total true strain rate V0 mmm-1 initial displacement speed nnn m-1 nominal engineering strain rate = v0/Lc (see 7.1 formula (1)) nemn m-1 average engineering strain rate = A/tf (see 7.5.3 equation (4)) (t) m-1 instantaneous engineering strain rate=de(t)/dt (see 7.5.3 equation (5)) pp m-1 average rate of uniform plastic strain. de(t)/dt at the beginning of yield or 1% strain to the strain range at the maximum force Average (see 7.5.4 equation (6)) Fu Hz test system upper frequency limit (force or displacement) Fn N maximum force stress R MPa engineering stress sigma MPa true stress Yield strength - specified plastic elongation - tensile strength Yield strength under Rep MPa Rp MPa specifies plastic elongation strength Rn MPa tensile strength Elastic modulus-stress strain curve slope E MPa elastic modulus T/CSAE XX-XXXX
Table 1 Symbols and descriptions (continued)
Slope of the elastic portion of the mE MPa stress-strain curve Note. 1, 1MPa = 1N/mm2; 2, under certain conditions (high resolution, two-way uniform extensometer, accurate calibration of the sample, etc.), elastic part the slope value of the stress-strain curve is consistent with the elastic modulus value.
4 Principle
Most materials exhibit varying degrees of strain rate sensitivity during deformation. Higher in height than described in GB/T 228.1 at the strain rate, in order to obtain a reliable stress-strain curve, the force and the elongation of the sample's original gauge length L0 must be measured to meet some additional conditions of. Through the test of this standard, the stress and strain of the force balance during plastic deformation can be obtained, and the maximum strain rate of the test is 103s-1.
5 Test equipment
The test equipment should meet the test requirements and maintain a constant strain rate throughout the test. The strain rate is less than 1s-1 when the test equipment should be closed-loop controlled; when the strain rate is greater than 1s-1, the control method of the test equipment can adopt open-loop control, but should Special measures are taken to keep the strain rate during the test constant and within acceptable limits. For this standard the recommended sample can be a hydraulic servo driven drop motion unit, flywheel impact, drop hammer and other systems.
The test equipment involved in this standard is constructed according to the principle of conservation of kinetic energy. The kinetic energy required for the test is the impact load of the specimen.
One side is produced and supplied (as shown in Figure A.1 of Appendix A), and the load sensing element is located on the side of the specimen holding fixture (see Figure A.1 in Appendix A).
In order to prevent the test error caused by the bending moment, the experimental process needs to ensure the coaxiality of the axisymmetric parallel sample and the loading rod. load the coaxiality of the rod can be determined by reference to ASTM E 1012. From a mechanical point of view, the loading rod should be fastened and easily controlled, and should be as the test loading system has a higher natural frequency and enables a shorter acceleration time.
6 Sample
6.1 Sample size
In this standard, a flat metal sheet should be selected for dynamic tensile test. The sampling position can be referred to GB/T 2975. Test equipment in addition to the loading speed that can be provided, the sample size is very important for the strain rate required for the experiment. The shorter the parallel length of the sample, the higher the strain rate that can be achieved by the test. The sample size requirements shall meet the requirements of Figure 1, and the parallel section length Lc of the sample shall satisfy Keep the gauge length L0 within the uniaxial tension state, and the parallel length Lc, width b0, thickness a0 and transition arc r of the sample should be Meet the following requirements.
- L0/b0 >= 2
- Lc >= L0 b0/2
- b0/a0 >= 2
- b0/bk <= 0.5
- r >= 10
Note. bk is the width of the sample holding end, and the dimensional tolerance of the sample is ±0.2mm.
T/CSAE XX-XXXX
Figure 1 Size of the sample
Note 1. When the strain rate reaches 103s-1, in order to obtain the force balance at the low strain (at the beginning of the test), it is necessary to select a suitable sample length.
Note 2. In addition to the sample size in Figure 1 and Appendix C, the shape and size of the sample may also be determined by mutual agreement, but should be noted in the test report.
The design of the clamping part of the specimen shall be carried out according to the requirements of the clamping part of the equipment, but shall be such that the clamping end of the specimen is not plastic during the test.
Deformation occurs.
If the force test is carried out by attaching the strain gauge to the specimen (Fig. 1), the design of the specimen size should be reserved.
Force measurement area. The force measurement area should be located in the region where the sample is not accelerated, and only elastic deformation occurs during the test.
Specimens for high-speed tensile tests shall be quasi-statically tested and the properties of the materials obtained shall be tested in accordance with GB/T 228.1.
Compare the material properties obtained with the standard equipment. The stress-strain curves obtained from these tests shall be allowed in the GB/T 228.1 standard.
The strain rate is carried out.
Since the automobile assembly or parts undergo work hardening after varying degrees of plastic deformation during service, the raw materials the dynamic mechanical properties differ from the dynamic mechanical properties of actual parts or plastically deformed materials (raw materials and pre-requisites) for a comparison of dynamic mechanical properties after the change, see Appendix B). If you want to consider the mechanical path or material deformation state, the mechanics of high strain rate of the material.
The effect of performance, can first process the appropriate size of the sample for different process paths or directly sample from the parts, but regardless of the choice the sampling method should ensure that the final test sample is the standard sample size.
6.2 Sample processing
The processing of the sample is based on the requirements in Appendix B of GB/T 228.1. The processing of the sample should pay special attention to prevent work hardening.
EDM corrosion cutting, water injection cutting, etc. to reduce the work hardening of the edge of the sample.
Note 1. If it is necessary to test the mechanical properties at a high strain rate for non-plate metal materials or metal sheets with a thickness greater than 3 mm, both sides may be tested.
Negotiate to determine the test plan.
6.3 Sampling
Samples should be sampled in the rolling direction unless otherwise agreed. During the test preparation, each strain rate should be guaranteed to be at least 3 Sheet sample. The sampling position of the sample can be referred to GB/T 2975.
T/CSAE XX-XXXX
7 Test requirements
7.1 Rate selection
Before testing the mechanical properties of the material at high strain rate, the initial displacement velocity v0 of the actuator should be reasonably selected to ensure the sample is tested to achieve the desired strain rate. The initial displacement velocity v0 can be determined by the formula (1) the variable rate is estimated to be. e = v0/Lc(1) in the formula (1), Lc is the length of the parallel segment of the sample. The strain rate during the test may vary due to the coaxiality of the actuator.
Note. For the drop weight structure test system, the initial displacement velocity v0 can be calculated from the drop height calculated according to the nominal strain rate reached by the test.
The strain rate of the parallel section of the specimen has a decisive influence on the mechanical behavior of the material. Therefore, the test should ensure that the samples are parallel the strain rate of the segment is constant rather than ensuring a constant loading speed of the actuator.
7.2 Force measurement
As the displacement velocity increases, the load at high strain rates will spontaneously transfer to the specimen, causing the vibration of the specimen and equipment components to increase.
plus. These vibrations can be either axial or bending vibrations. The vibration signal superimposed during the test is recorded in the force signal, from it appears on the stress-strain curve. In addition, during the deformation process (Rüders strain), the inherent vibration of the material will also be related to the force signal.
When a superposition occurs, a "power shock" phenomenon may also occur.
It is important to reduce or prevent vibration in the force signal when selecting the force measurement method. In general, the location of the force measurement is away from the test gauge length.
The further the position or the higher the speed of the device actuator, the greater the vibration generated by the test.
When the strain rate is less than or equal to 50s-1, the natural frequency of the piezoelectric sensor of the device is sufficient to meet the accuracy of the force measurement, and can be used.
The piezoelectric sensor of the device is used to measure the load; when the strain rate is greater than 50s-1, it is recommended to use in the pure elastic deformation zone of the sample.
The strain gauge (measured area, see Figure 1) or the force measurement by a local dynamometer.
Note 1. If the strain gauge is not used in the area where the specimen is only elastically deformed due to the equipment fixture, the strain gauge can be attached to the fixture ([1], [2], [3], [4]), However, the position of the clamp should be as small as possible from the gauge position of the specimen.
Note 2. If it is necessary to distinguish the vibration part caused by bending and twisting, the strain gauge can be attached on both sides of the sample to analyze the signal of the strain gauge separately, so as to identify the letter.
The part caused by the bending and twisting in the number, and overlapped by the strain gauge bridge to eliminate the oscillation caused by the bending and twisting.
Note 3. During the test, care should be taken to use the damping element on the loading rod to reduce the vibration, because the use of the damping element will reduce the initial strain of the test.
The rate, which affects the accuracy of the yield strength of the test material.
Calibration of the dynamometer can be performed on specimens with strain gauges under quasi-static conditions. When the calibration factor is obtained, it is applied to the sample.
The maximum stress value shall be no greater than 2/3 of the yield strength or the specified shape extension strength of the material. Other methods of force calibration can be found in the literature [1], [5], [6].
When the strain rate is less than 10s-1, the upper frequency limit fu(-3dB) should be at least 1kHz. For higher strain rates, it should be used Equation (2) determines the upper frequency limit of the force measurement system fu. fu >= 100 × e (2) the acquisition method, load and displacement/strain collection should be synchronized.
7.5 Data processing
7.5.1 Stress-strain curve
Force, extension, strain and stress-strain curves were processed in a similar manner to the GB/T 228.1 quasi-static tensile test.
The stress-strain curve of the material should be calculated from the raw measurement signal during the test. Monotonically increasing during the test the strain signal facilitates further analysis of the test data. If the measurement technique is used (such as signal clutter), monotony cannot be obtained.
The increased signal can be obtained by different program processing (such as using the moving average program, polynomial approximation, polynomial transfer).
Change or filter processing, etc.). If other measurement factors also affect the signal (such as speed reduction, etc.), it is necessary to check the test process.
Variable rate changes. The oscillation phenomenon and treatment method of the stress-strain curve appearing during the test should be explained.
In the determination of the key parameters of the material and the stress-strain-curve used for finite element calculation, the stress-strain curve needs to be smoothed.
It can usually be performed by moving average method, polynomial approximation, polynomial piecewise approximation or filtering. Smoothing the selection depends on different preconditions, such as the composition of the curve, the magnitude of the vibration, or the distribution and number of measurements. In short, smoothing Dealing with the risk of loss of information or subjective impact, the test report should indicate whether the data has been smoothed or in what way Reason.
Note. Before processing such as filtration and smoothing, optimize the equipment parameters such as fixture, buffer, and the coaxiality of the transmission rod to obtain a better original number.
according to.
T/CSAE XX-XXXX
7.5.2 Determination of key parameters
The key parameters of the tensile test of the material at high strain rate are determined by the stress-strain curve. Refer to the relevant terms of GB/T 228.1.
And definitions, the key parameters mainly include the lower yield strength ReL, the specified shape extension strength Rp, the tensile strength Rm, the maximum force plasticity Elongation of elongation Ag and elongation after fracture A.
The specified shape extension strength Rp can be calculated in the same manner as Rp0.2 at a plastic strain of 0.2% (consistent with GB/T 228.1).
In addition, the strength values for higher plastic strains should be marked with strain (eg 1%, 2%, 3%). In the case of uncertainty, such as high vibration amplitude Degree (greater than 5% of Rm), the calculation of Rp0.2 should be omitted, and the specified shaping extension strength at the higher variable speed value, such as the gauge of Rp3, should be recorded.
The plastic extension strength. The uncertainty in measuring the specified shape extension strength decreases as the vibration amplitude decreases.
The lower yield strength ReL corresponding to the upper yield strength is a key material parameter during the high speed tensile test. according to According to GB/T 228.1, ReL is defined as the average value of the stress during plastic yielding before the start of work hardening. When the force signal vibration is not guaranteed in the reliability of ReL, the strength corresponding to high plastic strain should be used instead of ReL.
As in Section 7.5.1, the tensile strength Rm is expressed as the maximum value of the stress-strain curve. The total elongation at the maximum force Agt is with GB/T 228.1 the definition in the quasi-static tensile test is similar to the strain value corresponding to the tensile strength of the material.
Consistent with the provisions of GB/T 228.1, the elongation after fracture is obtained from the gauge length on the measurement specimen and should be used preferentially on the specimen.
Pre-marking measures the elongation after break.
In addition, if the elongation of the gauge length L0 is measured by the conventional method of determining strain to fracture, the elongation after fracture can also be obtained from the stress-strain.
The break point on the curve is read. If the elongation after break is less than 5%, the elongation of the material can be obtained from the data on the stress-strain curve.
7.5.3 Determination of strain rate
In addition to calculating the nominal strain rate according to equation (1), the average strain rate during the test can be determined by the elongation at break A and the break.
The time required for cracking tf is calculated according to the following formula. emean = A/tf(4) Unlike the nominal strain rate, this parameter depends on the fit of the fixture or the deformability of the material. At the same time, the parameters and materials are the local strain rate of the neck region is not correlated.
The strain signal is differentiated from tim...
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 17 pages — is available in the English PDF.
How to Download T/CSAE 52-2016
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
T/CSAE 124.1-2020 — Automotive variable-displacement pendulum oil pump - Terminology
T/CSAE 124.2-2020 — Automotive variable-displacement pendulum oil pump - technical specification Drafting
T/CSAE 124.3-2020 — Automotive variable-displacement pendulum oil pump - Test method and device
T/CSAE 52-2016
$335.00