GB/T 40406-2021Standard test method for static modulus of elasticity and poisson's ratio of carbon materials in compression (English PDF)
炭素材料压缩静态弹性模量和泊松比测定方法
This is a limited preview
Buy now to download the full PDF (15 pages)
Need quotation for your management?
Get a formal quotation for GB/T 40406-2021 in 30 minutes.
Issued by
SAMR; SAC
Level / Type
National · Recommended
Issue date
August 20, 2021
Implementation date
March 1, 2022
Scope
GB/T 40406-2021 is the English-translated version of 炭素材料压缩静态弹性模量和泊松比测定方法.
GB/T 40406-2021 is the Chinese national test method for measuring the static modulus of elasticity and Poisson's ratio of carbon materials loaded in compression at room temperature.
It defines both quantities and lists the apparatus, including a drying oven, a vernier caliper and the adhesive for the strain gauges. Samples are cylinders 20 mm in diameter and 75 mm long, washed, dried at 105 °C and cooled before testing, two at a time.
The test steps cover measuring the diameter, pasting two-way strain gauges and soldering their wires, then recording longitudinal and transverse strain at six load values starting from 6000 N. The document closes with the calculation of results and the content of the test report. It was issued on 20 August 2021 and has applied since 1 March 2022.
Found what you need?
Document preview — GB/T 40406-2021
National Standard of the People's Republic of China
- ICS
- 29.050
- Classification
- Q 50
Issued by: State Administration for Market Regulation; Standardization Administration of the PRC
Contents
- Foreword3
- 1 Scope4
- 2 Normative references4
- 3 Terms and definitions4
- 4 Method summary5
- 5 Apparatus5
- 6 Samples6
- 7 Test steps6
- 8 Calculation of the results8
- 9 Test report9
1 Scope
This document specifies the relevant content of determination of the static modulus of elasticity and poisson's ratio of carbon materials in compression, such as the terms and definitions, method summary, apparatus, samples, test steps, calculation of results, the content of the test report, etc.
This document is applicable to the determination of the static modulus of elasticity and poisson's ratio of carbon materials in compression at room temperature.
2 Normative references
The following documents are essential to the application of this document. For the dated documents, only the versions with the dates indicated are applicable to this document; for the undated documents, only the latest version (including all the amendments) is applicable to this standard.
GB/T 8170 Rules of rounding off for numerical values and expression and judgement of limiting values
3 Terms and definitions
The following terms and definitions apply to this document.
3.1 Static modulus of elasticity
The modulus of elasticity measured by the static method is a measure between the stress and the elastic deformation from the material being elongated or compressed under the action of an external force.
Note: The value is the absolute value of the ratio of the normal stress to the strain on the cross-section of the sample.
3.2 Poisson's ratio
5 Apparatus
5.4 Drying oven: the highest temperature is 300 °C, and the accuracy is ±5 °C.
5.5 Vernier caliper: measuring range 0 mm~200 mm, accuracy 0.02 mm.
5.6 Adhesive: It shall become a hard Adhesive after curing, such as 502 glue, etc.
5.7 Electric soldering iron, solder wire, PTFE film, fine sandpaper, tweezers, alcohol, etc.
6 Samples
6.1 Sizes: a cylindrical sample with a diameter of 20mm and a length of 75mm; machining accuracy ±0.1 mm. The sample shall be processed to be straight; the end faces of the cylinder shall be parallel to each other. The perpendicularity of the end faces to the length direction is within 0.001 mm/mm; the roughness is Ra6.3.
6.2 Requirements: There are no visible cracks, pits, or other defects in the sample patch position. The sample shall be placed in a glass container filled with distilled water or alcohol. After washing and removing the dust on the surface of the sample, take it out and place it in a clean tray; then put it in a drying oven at 105 °C ± 5 °C for 2 hours; eventually, store it in a desiccator to cool it to room temperature for measurement.
6.3 Quantity: Take 2 samples each time.
7 Test steps
7.1 Measurement of the sample's diameter
Measure 4 times along the axial direction at the position in the middle of the sample (at 4/5 of the total length of the sample); rotate the sample 90° for each measurement; take the average value to calculate the area under pressure; the measurement error of the average cross-sectional area is within 0.5%.
7.2 Paste the strain gauge
Take an appropriate amount of adhesive and apply it evenly on the surface of the position to be bonded; wipe the surfaces of the strain-gauges and terminals (binding posts) with the anhydrous ethanol cotton balls. After drying, apply a thin layer of adhesive. After the adhesive becomes thick, accurately paste the strain gauge's terminal on the surface of the sample, and cover it with a layer of PTFE film. Then, use your fingers to squeeze out the excess adhesive along the longitudinal direction of the strain gauge and discharge the bubbles in the adhesive layer.
Do not touch the surface of the strain gauge with your hands during the entire operation; the two-way strain gauge shall be perpendicular or parallel to the force direction; the adhesive layer cannot have bubbles and impurities; the sensitive grid of the strain gauge cannot be broken or deformed.
In order to prevent the pasted strain gauge from moisture, corrosion, and mechanical damage, certain protective measures shall be taken for the strain gauge.
Note: In order to ensure a firm bonding, after applying a certain pressure on the PTFE film, carry out curing and stabilization treatment according to the temperature, time, and pressure indicated in the manual of the adhesive.
7.3 Welding of the strain gauge's wire
7.3.1 The strain gauge patch is pasted on the sample, after curing and stabilization treatment, the wire can be welded.
7.3.2 Use fine sandpaper to lightly polish solder feet and terminals of the strain gauge, to remove the adhesive and oxide layer on their surfaces.
7.3.3 Coat the soldering flux on the surfaces of the strain gauge's solder feet and the terminals; use an electric soldering iron to melt the solder wire, then weld to let the solder feet be connected with the terminals through the wire.
7.4 Measurements of stress and strain
7.4.1 For the welded sample, use the 1/4 bridge and common compensation wiring method, to connect the sample and the common compensation wire to the dynamic and static resistance strainmeter. Then, place the tested sample vertically on the compression platform of the universal material testing machine.
7.4.2 Measure 6 load values and the corresponding strains for each sample.
The starting point of the load value shall be 6000 N (to ensure that the sample has a certain longitudinal and transverse strain); measure and record the sample's longitudinal strain epsilon longitudinal and transverse strain epsilon transverse at the load.
Then, for every 1000 N added, respectively measure and record the corresponding longitudinal strain epsilon longitudinal and transverse strain epsilon transverse. The testing machine continuously loads without impact at a speed of 3 kN/cm² per minute; the maximum load value is 40%~85% (11000N) of the pressure-bearing capacity (breaking strength) of the same material with the same diameter. […]
......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 15 pages — is available in the English PDF.
Referenced standards
Similar standards
How to Download GB/T 40406-2021
- 1
Add to cart
Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.
- 2
Checkout
Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).
- 3
Fast delivery
After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.
- 4
Invoice included
A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.
Related Standards
GB/T 8170-1987 — Rules for rounding off of numerical values
GB/T 8170-2008 — Rules of rounding off for numerical values & expression and judgement of limiting values
GB/T 10003-2026 — Biaxially oriented polypropylene (BOPP) film
GB/T 40406-2021