Valid

GB/T 36228-2018Non-destructive testing—Guide for plannar flaw height sizing by ultrasonic testing (English PDF)

无损检测 平面型伤高度超声定量导则

Preview PDF

This is a limited preview

Buy now to download the full PDF (24 pages)

Need quotation for your management?

Get a formal quotation for GB/T 36228-2018 in 30 minutes.

Issued by

SAMR; SAC

Level / Type

National · Recommended

Issue date

May 14, 2018

Implementation date

December 1, 2018

Scope

GB/T 36228-2018 is the English-translated version of 无损检测 平面型伤高度超声定量导则.

GB/T 36228-2018 is a guide to measuring the height of planar flaws in ferritic and austenitic workpieces by ultrasonic testing.

It describes the principles and techniques that size a flaw from the time of flight of the ultrasonic signal or from a time-of-flight difference: the 30-70 method, the tip diffraction method, and the twin-crystal bi-modal and twin-crystal same-mode techniques.

It defines terms such as the bi-modal method, corner reflection, doublet, far surface and near surface, and it gives the limitations of each method and an evaluation procedure for flaw height in two informative annexes.

The guide does not cover sizing by signal amplitude, the measurement of flaw length or acceptance criteria. Inspection bodies and NDT laboratories use it. It was issued on 14 May 2018 and has applied since 1 December 2018.

Found what you need?

Document preview — GB/T 36228-2018

National Standard of the People's Republic of China

ICS
19.100
Classification
J 04

Issued by: State Administration for Market Regulation; Standardization Administration of the PRC

Contents

  • Foreword
  • 1 Scope
  • 2 Normative references
  • 3 Terms and Definitions
  • 4 Method Summary
  • 5 30-70 Method
  • 6 endpoint diffraction method
  • 7 twin crystal double mode
  • 8 twin crystal isomorphism
  • Appendix A (informative) Limitations of the method
  • Appendix B (informative) Damage Assessment Process

Foreword

This standard was drafted in accordance with the rules given in GB/T 1.1-2009.

1 Scope

This standard specifies the ultrasonic testing technology and its principle for determining the height of the flat surface of the ferrite and austenite workpieces. this The standard recommends the use of time-of-flight (TOF) or propagation time difference (deltaTOF) for ultrasonic height quantification.

The flat-type injury height quantitative techniques described in this standard have their best application range. See Appendix A for details.

This standard recommends the determination of the height of the flat injury according to the evaluation procedure in Appendix B.

This standard does not apply to the method of quantifying the size of the injury using the signal amplitude method, and does not involve the method of quantification of the length of the flat injury. Acceptance criteria for type injuries.

2 Normative references

The following documents are indispensable for the application of this document. For dated references, only dated versions apply to this document. For undated references, the latest edition (including all amendments) applies to this document.

GB/T 12604.1 Non-destructive testing terminology ultrasonic testing

GB/T 20737 General Terms and Definitions for Nondestructive Testing

3 Terms and definitions

The following terms and definitions as defined in GB/T 12604.1 and GB/T 20737 apply to this document.

3.1 Bi-modal method

An ultrasonic detecting method for quantitatively determining the height of a wound by using both longitudinal and transverse waves existing in a workpiece.

3.2 Corner reflection

The ultrasonic beam is obliquely propagated to the 90° interface formed by the surface of the wound and the workpiece to be inspected, due to the interaction of the acoustic wave and the interface. The raw ultrasound energy is reflected.

3.3 Doublet

Simultaneously appear in pairs on the screen, and two signals that move synchronously as the probe approaches and moves away from the injury.

Note: When the height of the injury is quantified by the endpoint diffraction method, the end point signal and the lower end point signal (or the end angle reflection signal) are double peaks.

3.4 Far surface

At the time of inspection, the other surface of the workpiece to be inspected is opposite to the probe contact surface.

Note: For example, when the pipe is inspected from the outer surface, the inner surface of the pipe is the far surface.

3.5 Near surface

The surface of the workpiece to be in contact with the probe during inspection.

Note: For example, when the pipe is inspected from the outer surface, the outer surface of the pipe is the near surface.

......
This preview omits tables, figures, formulas and parts of the technical clauses. The complete document — 24 pages — is available in the English PDF.

Referenced standards

Similar standards

How to Download GB/T 36228-2018

  1. 1

    Add to cart

    Click "Download PDF" on this page and choose "Buy this standard". You can add more standards before checkout.

  2. 2

    Checkout

    Enter your email and billing details. Payment is processed securely by Stripe (cards or bank transfer). Prefer bank details? Request a quotation (min. order $300).

  3. 3

    Fast delivery

    After payment you'll receive an email confirmation. The English PDF is sent to the same address, usually within minutes and at the latest within 1 business day.

  4. 4

    Invoice included

    A tax invoice is attached to the confirmation email. Need a custom invoice? Contact us.

Related Standards

English PDF
24 pages
Fast delivery
Invoice included
View Cart

Secure payment via Stripe

Payments accepted

VisaMastercardAmerican ExpressApple PayGoogle PayStripe

GB/T 36228-2018

$415.00